PROVIDING DUPLEX AND SUPER DUPLEX STEEL PRODUCTS SINCE 1975

The word "Hastelloy" describes a class of nickel-based, corrosion-resistant metal alloys. When compared to conventional alloys, Hastelloy offer a much higher level of corrosion resistance due to a special mix of characteristics. The melting point of Hastelloy is greater. Often used for chemical and acid applications, Hastelloy Alloy is a very robust nickel alloy that resists corrosion.

Hastelloy Alloy, Hastelloy Metal, Hastelloy X, Hastelloy Material, Hastelloy C4, Hastelloy Price Per Kg, Hastelloy Uses, Hastelloy Price, Hastelloy Composition.

Hastelloy Metal Alloys, Hastelloy Material Properties, Hastelloy Alloy Composition, Hastelloy Material Grades, Hastelloy Hardness, Hastelloy C 2000 Alloy.

With the addition of chromium and molybdenum, the material is corrosion-resistant and high-temperature resistant. Since Hastelloy Metal is ductile, it may be easily produced. A variety of pipes, exchangers, vessels, and valves are made from Hastelloy, particularly for use in the chemical and petrochemical industries.


Types of Hastelloy

Hastelloy Equivalent Material

EU
EN
USA
-
Germany
DIN,WNr
Japan
JIS
France
AFNOR
Russia
GOST
NiMo16Cr15W C276 2.4819 NW 0276 - ХН65МВУ
NiCr21Mo14W C22 2.4602 NW 6022 NU-30M -

Hastelloy Cost, Hastelloy Types, Hastelloy Density, Hastelloy ASTM, Hastelloy Melting Point, Hastelloy Compatibility Chart, Hastelloy at Best Price in India.

If you are looking for best prices for Hastelloy, Hastelloy Alloy Material email us on info@duplexsteelalloys.com or call us on +91 9664408767

Hastelloy ASTM Grades

Sheet / Plate Pipe Buttweld Fittings Flanges Forged Fittings Fasteners Bars
ASTM B575, B333 ASTM B619, B622 ASTM B366 ASTM B564 ASTM B564 ASTM B574 ASTM B574, B335

Hastelloy Chemical Composition

Grade C Mn Si S Co Ni Cr Fe Mo P
C22 0.010 max 0.50 max 0.08 max 0.02 max 2.50 max 50.015 min* 20.00 – 22.50 2.00 – 6.00 12.50 – 14.50 0.02 max
C276 0.010 max 1.00 max 0.08 max 0.03 max 2.50 max 50.99 min* 14.50 – 16.50 4.00 – 7.00 15.00 – 17.00 0.04 max
B2 0.010 max 1.00 max 0.08 max 0.03 max 2.50 max 50.99 min* 14.50 – 16.50 4.00 – 7.00 15.00 – 17.00 0.04 max
Grade Ni Mo Cr Fe W Mn C Al Ti Si
B3 65.0 min 28.5 1.5 1.5 3.0 max 3.0 max 0.01 max 0.50 max 0.2 max 10 max
Grade Ni Mo Cr Fe Mn C Co Si P S
X Balance 8.00 – 10.00 20.50 – 23.00 17.00 – 20.00 1.00 max 0.05 – 0.15 0.50 – 2.50 1.00 max 0.04 max 0.03 max

Hastelloy Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Hastelloy C22 8.69 g/cm3 1399 °C (2550 °F) Psi – 1,00,000 , MPa – 690 Psi – 45000 , MPa – 310 45 %
Hastelloy C276 8.89 g/cm3 1370 °C (2500 °F) Psi – 1,15,000 , MPa – 790 Psi – 52,000 , MPa – 355 40 %
Hastelloy B2 8.89 g/cm3 1370 °C (2500 °F) Psi – 1,15,000 , MPa – 790 Psi – 52,000 , MPa – 355 40 %
Hastelloy B3 9.2 g/cm3 1370 °C (2550 °F) Psi – 1,15,000 , MPa –760 Psi – 52,000 , MPa – 350 40%
Hastelloy X 8.22 g/cm³ 1355°C 655 MPa 240 MPa 35%

Hastelloy Physical Properties

Physical Property British Units Metric Units
Density RT 0.321 lb/in3 RT 8.89 g/cm3
Electrical Resistivity RT 48.4 μohm.in RT 1.23 μohm.m
200°F 48.7 μohm.in 100°C 1.24 μohm.m
400°F 49.0 μohm.in 200°C 1.25 μohm.m
600°F 49.5 μohm.in 300°C 1.26 μohm.m
800°F 49.8 μohm.in 400°C 1.26 μohm.m
1000°F 50.6 μohm.in 500°C 1.28 μohm.m
- - 600°C 1.30 μohm.m
Thermal Conductivity 100°F 71 Btu.in/h.ft2.°F 50°C 10.5 W/m.°C
200°F 77 Btu.in/h.ft2.°F 100°C 11.2 W/m.°C
400°F 90 Btu.in/h.ft2.°F 200°C 12.9 W/m.°C
600°F 104 Btu.in/h.ft2.°F 300°C 14.7 W/m.°C
800°F 117 Btu.in/h.ft2.°F 400°C 16.5 W/m.°C
1000°F 132 Btu.in/h.ft2.°F 500°C 18.3 W/m.°C
Mean Coefficient of
Thermal Expansion
75-200°F 6.2 μin/in.°F 24-100°C 11.2 μm/m.°C
75-400°F 6.7 μin/in.°F 24-200°C 12.0 μm/m2.°C
77-600°F 7.1 μin/in.°F 24-300°C 12.7 μm/m.°C
77-800°F 7.3 μin/in.°F 24-400°C 13.1 μm/m.°C
77-1000°F 7.4 μin/in.°F 24-500°C 13.3 μm/m.°C
77-1100°F 7.8 μin/in.°F 24-600°C 13.8 μm/m.°C
Magnetic Permeability 200 oersted 1.0002 15.9 kA/m 1.0002
Specific Heat RT 0.102 Btu/lb.°F RT 427 J/kg.°C
Dynamic Modulus
of Elasticity
RT 29.8 x 106psi RT 205 GPa
400°F 28.3 x 106psi 200°C 195 GPa
600°F 27.3 x 106psi 300°C 189 GPa
800°F 26.4 x 106psi 400°C 183 GPa
1000°F 25.5 x 106psi 500°C 178 GPa
Melting Range 2415-2500°F - 1323-1371°C -
Poisson’s Ratio - - RT 0.31